Emery wear-hardened floor_ Z-lion Diamond Tools Group

Welcome To ZL DIAMOND TECHNOLOGY CO.,LTD.

Emery wear-hardened floor


Emery wear-resistant hardened floor refers to sprinkle emery aggregate on the ground at the beginning of making the floor, and construct according to the process of emery wear-resistant floor.  After curing for 28 years, use hardener and penetrant to infiltrate the ground. 10-30mm, form a layer of high-strength and high-hard polycrystalline silicide, establish a solid, impermeable dense body for the floor, form a dense, hard, wear-resistant surface layer, with excellent wear resistance and good wear resistance. Shock resistance, heavy load capacity 

Emery wear-resistant hardened floor refers to sprinkle emery aggregate on the ground at the beginning of making the floor, and construct according to the process of emery wear-resistant floor. After curing for 28 years, use hardener and penetrant to infiltrate the ground. 10-30mm, form a layer of high-strength and high-hard polycrystalline silicide, establish a solid, impermeable dense body for the floor, form a dense, hard, wear-resistant surface layer, with excellent wear resistance and good wear resistance. Shock resistance, heavy load capacity

1. Clean the ground, use a polishing machine to wipe and compact it, and then polish and remove white alkali and floating dust on the surface after at least 15 days of maintenance. For gold steel sand hardener floors or old concrete floors, remove oil, paint and loose structures from the surface that affect infiltration, and then thoroughly clean the floor.

2. For the old ground that is too dry, use clean water to fully wet the floor surface.

3, the use of hardener fully wet the pre-treated emery surface, and keep wet for 1-2 hours. During this period should use brush, mop or roller tools such as constant friction surface, so that the hardener can more effectively infiltrate into the emery interior.

4, when the temperature is higher, the surface of the hardener because of water evaporation reasons quickly become sticky, can be sprayed with a small amount of water to dilute the thickened hardener, but the amount should not be too much.

5, remove residual liquid: use plastic scraper or mop to clean the remaining liquid on the surface, can also be washed with a lot of water, but need to pay attention to the phenomenon of water immersion.

6, maintenance: dry 24 hours after the ground can walk open, normal use should be seven days after maintenance and then put into use. Permeable hardener active components gradually react with cement, frequent use of wet mop cleaning the ground can promote permeable into the emery internal gel to continue to react, can obtain strength and gloss earlier.

7, polishing: the finished ground will become more and more bright with the frequent friction of the use of time, but also immediately after finishing with mechanical artificial polishing, in order to get a certain gloss floor effect.



Chat now